Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, TD = 8.30 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
ASTM D 882
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin
FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou..
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
ASTM D882
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
ASTM D882
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera..
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
ASTM D882
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u..
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Next Generation DOWLEX® NG 3347A resin with extra stretch performance (ESP)is an ethylene-octene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. DOWLEX NG 33..
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Film Tensile Strength at Yield, TD 8.30 - 12.0 MPa
1200 - 1740 psi
Average value: 9.92 MPa Grade Count:28
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..
Copyright © lookpolymers.com All Rights Reserved