Polymer Property : Film Tensile Strength at Yield, TD = 711 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 4.90 MPa
711 psi
ASTM D882
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light..
Film Tensile Strength at Yield, TD 4.90 MPa
711 psi
ISO 527-3
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st..