Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 44.0 MPa | 6380 psi | ASTM D882 |
Eastman Eastar 5445 PCTG Copolyester, Film
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |