Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyester, TP , Polycyclohexylenedimethylene Terephthalate (PCT) , Glycol-Modified PCT (PCTG) Copolyester
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is transparent. It is tough and resistant to stress whitening. It has fast forming cycles and is easy to form. Eastar PCTG Copolyester 5445 is sterilizable by both gamma radiation and ethylene oxide (ETO) methods. Its scrap can be reused.Applications/UsesBagsCredit cardsGaming cardsIdentification cardsPlastic CardsRigid medicalBlister packagingDebit cardsGift cardsPhone cardsRapid deployment flood wallsSmart cardsKey AttributesExcellent clarityEffective barrier propertiesExcellent colorabilityGood stiffnessSterilizable with ethylene oxide, electron beam, and gamma rays
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D1505
Melt Density 1.08 g/cc

@Temperature 285 °C
0.0390 lb/in³

@Temperature 545 °F
ASTM D1238
Water Vapor Transmission 7.00 g/m²/day
0.451 g/100 in²/day
ASTM F372
Oxygen Transmission 11.0 cc-mm/m²-24hr-atm
27.9 cc-mil/100 in²-24hr-atm
ASTM D3985
Carbon Dioxide Transmission 49.0 cc-mm/m²-24hr-atm
124 cc-mil/100 in²-24hr-atm
ASTM D1434
Thickness 250 microns
9.84 mil
ASTM D374
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 45.0 MPa
6530 psi
ASTM D882
Film Tensile Strength at Yield, TD 44.0 MPa
6380 psi
ASTM D882
Tensile Modulus 1.60 GPa
232 ksi
TD; ASTM D882
1.60 GPa
232 ksi
MD; ASTM D882
Coefficient of Friction 0.50
0.50
ASTM D1894
Elmendorf Tear Strength, MD >= 12.0 g/micron
>= 305 g/mil
ASTM D1922
Elmendorf Tear Strength, TD >= 12.0 g/micron
>= 305 g/mil
ASTM D1922
Dart Drop 1.84 g/micron
46.7 g/mil
23°C; ASTM D1709
2.16 g/micron
54.9 g/mil
at -18°C; ASTM D1709
Film Tensile Strength at Break, MD 57.0 MPa
8270 psi
ASTM D882
Film Tensile Strength at Break, TD 53.0 MPa
7690 psi
ASTM D882
Thermal Properties Metric English Comments
Specific Heat Capacity 1.09 J/g-°C

@Temperature 10.0 °C
0.261 BTU/lb-°F

@Temperature 50.0 °F
DSC
1.14 J/g-°C

@Temperature 30.0 °C
0.272 BTU/lb-°F

@Temperature 86.0 °F
DSC
1.64 J/g-°C

@Temperature 100 °C
0.392 BTU/lb-°F

@Temperature 212 °F
DSC
1.86 J/g-°C

@Temperature 180 °C
0.445 BTU/lb-°F

@Temperature 356 °F
DSC
2.16 J/g-°C

@Temperature 290 °C
0.516 BTU/lb-°F

@Temperature 554 °F
DSC
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ASTM C177
Glass Transition Temp, Tg 87.0 °C
189 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.56
1.56
n<sub>D</sub>; ASTM D542
Haze 1.0 %
1.0 %
ASTM D1003
Gloss 98 %
98 %
at 60°; ASTM D2457
Transmission, Visible 91 %
91 %
Total Transmittance; ASTM D1003