Film Tensile Strength at Yield, TD 6.21 MPa
900 psi
at 2% offset; ASTM D882
ExxonMobil LD 135.09 Cast Packaging Film Resin  (discontinued **)
LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging..
Film Tensile Strength at Yield, TD 6.21 MPa
900 psi
at 2% offset; ASTM D882
ExxonMobil Escorene® LD 712.06 Film Resin  (discontinued **)
Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular..
Film Tensile Strength at Yield, TD 6.21 - 15.9 MPa
900 - 2300 psi
Average value: 10.9 MPa Grade Count:140
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..