Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 53.0 MPa | 7690 psi | ASTM D882 |
Eastman 9921P PET Film
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Film Tensile Strength at Yield, TD | 53.0 MPa | 7690 psi | ASTM D638 |
Wanshijie APET Sheet APET sheet is one of the earliest plastic sheets our company develops and produces. It has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce .. |
|||
Film Tensile Strength at Yield, TD | 53.0 - 265 MPa | 7690 - 38400 psi | Average value: 206 MPa Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |