Polymer Property : Film Tensile Strength at Yield, TD = 50.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD >= 50.0 MPa
>= 7250 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer