Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 30.40 MPa | 4409 psi | ASTM D882 |
Dow INSPIRE™ D118.01 Developmental Performance Polymer D118.01 Developmental Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion. Film and sheet produced from this resin offer improved stiffness, heat resistance, .. |