Film Tensile Strength at Yield, TD 3.00 MPa
435 psi
ASTM D882
ExxonMobil Escorene® LD-713 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 15% vinyl acetate copolymer film resin. Film made from LD-713 exhibits very high impact strength, high clarity and excellent heat sealability.App..