Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 265 MPa | 38400 psi | Test speed 100%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 30 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for.. |