Film Tensile Strength at Yield, TD 24.1 - 41.4 MPa
3500 - 6000 psi
ASTM D882
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **)
Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc..
Film Tensile Strength at Yield, TD 24.1 MPa
3500 psi
ASTM D 882 A
Total Finathene® HL 328 HDPE resin  (discontinued **)
Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by ..