Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE/ECTFE, Molded/Extruded , Nylon
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistance, exceptional clarity and enhanced mechanical properties. It is widely used as a protective film for long term outdoor applications like retro-reflective signage and photovoltaic cells. Information provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.183 g/cc
1.183 g/cc
ASTM D1505
Density 1.77 g/cc
0.0640 lb/in³
Yield Density
Moisture Absorption at Equilibrium 0.0030 %
0.0030 %
ASTM D570
Water Vapor Transmission 12.92 g/m²/day
0.8320 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Thickness 30.5 microns
1.20 mil
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 70.3 - 82.0 MPa
10200 - 11900 psi
ASTM D882
Film Tensile Strength at Yield, TD 24.1 - 41.4 MPa
3500 - 6000 psi
ASTM D882
Film Elongation at Break, MD 130 - 160 %
130 - 160 %
ASTM D882
Film Elongation at Break, TD 390 - 520 %
390 - 520 %
ASTM D882
Film Elongation at Yield, MD 35 - 45 %
35 - 45 %
ASTM D882
Film Elongation at Yield, TD 15 - 17 %
15 - 17 %
ASTM D882
Secant Modulus, MD 1.338 - 1.53 GPa
194.1 - 222 ksi
ASTM D882
Secant Modulus, TD 0.765 - 0.830 GPa
111 - 120 ksi
ASTM D882
Coefficient of Friction 0.50 - 0.70
0.50 - 0.70
film to stainless steel; ASTM D1894
1.0 - 1.6
1.0 - 1.6
film to film; ASTM D184
Elmendorf Tear Strength, MD 32.8 - 39.4 g/micron
833 - 1000 g/mil
Elmendorf Tear Strength, TD 45.94 - 52.48 g/micron
1167 - 1333 g/mil
ASTM D1922
Film Tensile Strength at Break, MD 100 - 134 MPa
14500 - 19500 psi
ASTM D882
Film Tensile Strength at Break, TD 54.5 - 67.6 MPa
7900 - 9800 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 271 °C
520 °F
DTA
Oxygen Index 30 %
30 %
ASTM D2863
Shrinkage, MD -7.00 %
-7.00 %
302°F / 150°C - 10 min.; ASTM D1204
-3.00 %
-3.00 %
212°F / 100°C - 10 min.; ASTM D1204
Shrinkage, TD 1.0 %
1.0 %
212°F / 100°C - 10 min.; ASTM D1204
3.5 %
3.5 %
302°F / 150°C - 10 min.; ASTM D1204
Optical Properties Metric English Comments
Refractive Index 1.407
1.407
ASTM D542
Haze 1.5 - 4.5 %
1.5 - 4.5 %
ASTM D1003
Transmission, Visible 95 %
95 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Constant 2.6

@Frequency 1000 Hz
2.6

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149(A)