Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 34.0 MPa | 4930 psi | ASTM D882 |
ExxonMobil Escorene® HD-7745 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7745 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Film Tensile Strength at Yield, TD | 34.0 MPa | 4930 psi | ASTM D882 |
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Film Tensile Strength at Yield, TD | 34.0 MPa | 4930 psi | ASTM D882 |
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness... |