Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD >= 33.0 MPa
>= 4790 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD >= 33.0 MPa
>= 4790 psi
ASTM D882
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Film Tensile Strength at Yield, TD 33.0 MPa
4790 psi
ASTM D882
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness..
Film Tensile Strength at Yield, TD 33.0 MPa
4790 psi
ASTM D882
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness...