Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 19.3 MPa | 2800 psi | ASTM D882, A |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Film Tensile Strength at Yield, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin Product Description: Enable 35-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, TD | 19.3 MPa | 2800 psi | ASTM D882 |
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |