Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 9.70 - 23.2 MPa
1410 - 3360 psi
Average value: 14.0 MPa Grade Count:6
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..