Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | ASTM D 882 |
NOVA Chemicals Sclair® FP020-D Octene Copolymer LLDPE Film Resin FP020-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FP020.. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | ASTM D882 |
Westlake Mxsite LC78105-C Polyethylene Film, Using Energx Technology Services
(discontinued **) Mxsite LC78105-C polyethylene is recommended for the skin layers of blown stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cli.. |
|||
Film Tensile Strength at Yield, TD | 9.70 - 23.2 MPa | 1410 - 3360 psi | Average value: 14.0 MPa Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | ASTM D882 |
LyondellBasell Plexar® PX3227 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | |
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | |
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | |
Dow LDPE 526A Low Density Polyethylene, Blown Film Grade DOW LDPE 526A resin is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains medium levels of antiblock additive. .. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | |
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Film Tensile Strength at Yield, TD | 9.70 MPa | 1410 psi | |
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re.. |