Polymer Property : Film Tensile Strength at Yield, TD = 13600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 93.8 MPa

@Strain >=5.00 %
13600 psi

@Strain >=5.00 %
ASTM D882A
DuPont Teijin Films Melinex® 194 Polyester Film, 380 Gauge
Melinex® 194 is a non-pretreated, super clear, polyester film with balanced shrinkage.Also Available in 400 and 500 gaugeInformation provided by DuPont.