Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 194 Polyester Film, 380 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 194 Polyester Film, 380 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 194 is a non-pretreated, super clear, polyester film with balanced shrinkage.Also Available in 400 and 500 gaugeInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 93.1 MPa

@Strain >=5.00 %
13500 psi

@Strain >=5.00 %
ASTM D882A
Film Tensile Strength at Yield, TD 93.8 MPa

@Strain >=5.00 %
13600 psi

@Strain >=5.00 %
ASTM D882A
Film Tensile Strength at Break, MD 166 MPa
24100 psi
ASTM D882A
Film Tensile Strength at Break, TD 222 MPa
32200 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.4 %

@Temperature 190 °C,
Time 300 sec
1.4 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.2 %

@Temperature 190 °C,
Time 300 sec
1.2 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 0.20 %
0.20 %
ASTM D1003
Transmission, Visible 90 %
90 %
TLT; ASTM D1003
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved