Polymer Property : Film Tensile Strength at Yield, TD = 1270 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, TD 8.76 MPa
1270 psi
at 2% offset; ASTM D882
ExxonMobil LL 1235x70 Cast Film Resin  (discontinued **)
LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical