Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 180/1A |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |