Polymer Property : Shear Modulus = 96.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.662 GPa
96.0 ksi
Calculated
Uniseal BETABRACE™ 85001 Epoxy
BETABRACE™ 85001 is a composite used for reinforcing sheet metal. It is composed of a moderate temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85001 provides ..
Shear Modulus 0.662 GPa
96.0 ksi
Calculated
Uniseal BETABRACE™ 85002 Epoxy
BETABRACE™ 85002 is a composite used for reinforcing sheet metal. It is composed of a high temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85002 provides adhe..
Shear Modulus 0.662 GPa
96.0 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Modulus 0.662 GPa
96.0 ksi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..