Polymer Property : Shear Modulus = 9.62 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 9.62 GPa
1400 ksi
Calculated
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..