Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.46 - 5.98 GPa | 792 - 867 ksi | Average value: 5.76 GPa Grade Count:3 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |