Shear Modulus 5.88 GPa
853 ksi
Calculated
Plenco 5350 Phenolic, Granular, Compression Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...