Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.88 GPa | 853 ksi | Calculated |
Plenco 5350 Phenolic, Granular, Compression Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |