Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 80.7 GPa | 11700 ksi | |
Crucible Steel 420 and 420F Chromium Steel Crucible 416 Plus is a hardenable chromium steel which is the general purpose cutlery grade. This grade is magnetic in all conditions. Information provided by Crucible Specialty Metals. |