Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 45.0 GPa | 6530 ksi | calculated |
Schott N-LASF45 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 45.0 GPa | 6530 ksi | calculated |
Schott N-LAK10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 45.0 GPa | 6530 ksi | calculated |
Schott N-LAK34 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 45.0 GPa | 6530 ksi | calculated |
Schott N-LAK8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 45.0 GPa | 6530 ksi | |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |