Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.89 GPa | 419 ksi | Calculated |
Plenco 2000 Phenolic, Granular, Transfer Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |