Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.40 GPa @Temperature 130 °C |
348 ksi @Temperature 266 °F |
In-Plane, Wet; EN6031 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |