Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.70 GPa | 247 ksi | Calculated |
PolyOne Geon™ 83510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Shear Modulus | 1.70 GPa | 247 ksi | Average value: 1.70 GPa Grade Count:3 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |