Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.165 GPa | 24.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 1/4-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.165 GPa | 24.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 5/32-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.165 GPa | 24.0 ksi | Plate Shear, L Direction, typ, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Modulus | 0.165 GPa | 24.0 ksi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-36 - 1/8 - 4.5 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Modulus | 0.165 GPa | 24.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Modulus | 0.165 GPa | 24.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |