Polymer Property : Shear Modulus = 0.165 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.165 GPa
24.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Modulus 0.165 GPa
24.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 5/32-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Modulus 0.165 GPa
24.0 ksi
Plate Shear, L Direction, typ, preliminary value obtained at .500 inch thickness
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Modulus 0.165 GPa
24.0 ksi
Plate Shear, L Direction
Hexcel® HexWeb® HRH-36 - 1/8 - 4.5 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Modulus 0.165 GPa
24.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Modulus 0.165 GPa
24.0 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..