Mechanical Properties Metric English Comments
Shear Modulus 152 GPa
22000 ksi
Calculated
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Shear Modulus 152 GPa
22000 ksi
Calculated
CoorsTek AD-996 99.6% Alumina
Shear Modulus 152 GPa
22000 ksi
Calculated
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Shear Modulus 152 GPa
22000 ksi
Calculated
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Shear Modulus 152 GPa
22000 ksi
Calculated
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3)
Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..