Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.31 - 2.43 GPa | 335 - 352 ksi | Average value: 2.35 GPa Grade Count:3 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |