Polymer Property : Shear Modulus = 188 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 188 GPa
27300 ksi
calculated
Ceradyne CeraTrex™ SC-P2 Silicon Carbide
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company
Shear Modulus 188 GPa
27300 ksi
calculated
Ceradyne CeraTrex™ SC-P3 Silicon Carbide
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company