Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.840 GPa | 122 ksi | DIN 53457 |
Global PP-1142-R Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-disposable drinkware, thin-walled parts, medical applicationsInformation provided by Global Polymers Corporation. |