Polymer Property : Shear Modulus = 0.840 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.840 GPa
122 ksi
DIN 53457
Global PP-1142-R Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-disposable drinkware, thin-walled parts, medical applicationsInformation provided by Global Polymers Corporation.