Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.30 GPa | 189 ksi | calculated |
BASF Capron® 1202CQ Nylon 6 (Dry)
(discontinued **) Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava.. |
|||
Shear Modulus | 1.30 GPa | 189 ksi | in plane |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |