Mechanical Properties Metric English Comments
Shear Modulus 1.07 GPa
155 ksi
Calculated
Network Polymers Kepital® F30-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Shear Modulus 1.07 - 5.86 GPa
155 - 850 ksi
Average value: 3.20 GPa Grade Count:23
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Shear Modulus 1.07 GPa
155 ksi
Calculated
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix
HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F)..
Shear Modulus 1.07 GPa
155 ksi
Calculated
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
Shear Modulus 1.07 GPa
155 ksi
Calculated
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..