Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.07 GPa | 155 ksi | Calculated |
Network Polymers Kepital® F30-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Shear Modulus | 1.07 - 5.86 GPa | 155 - 850 ksi | Average value: 3.20 GPa Grade Count:23 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Shear Modulus | 1.07 GPa | 155 ksi | Calculated |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F).. |
|||
Shear Modulus | 1.07 GPa | 155 ksi | Calculated |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Shear Modulus | 1.07 GPa | 155 ksi | Calculated |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |