Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.893 - 0.932 GPa | 130 - 135 ksi | Calculated |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |