Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.750 - 0.930 GPa | 109 - 135 ksi | calculated |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |
|||
Shear Modulus | 0.893 - 0.932 GPa | 130 - 135 ksi | Calculated |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |