Mechanical Properties Metric English Comments
Shear Modulus 0.350 - 4.00 GPa

@Temperature 0.000 - 350 °C
50.8 - 580 ksi

@Temperature 32.0 - 662 °F
Average value: 1.75 GPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..