Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0768 - 4.00 GPa @Temperature -50.0 - 350 °C |
11.1 - 580 ksi @Temperature -58.0 - 662 °F |
Average value: 2.35 GPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Shear Modulus | 0.350 - 4.00 GPa @Temperature 0.000 - 350 °C |
50.8 - 580 ksi @Temperature 32.0 - 662 °F |
Average value: 1.75 GPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |