Polymer Property : Shear Modulus = 0.0725 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.000500 GPa
0.0725 ksi
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber..