Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.000500 GPa | 0.0725 ksi | |
Natural Rubber, Vulcanized (NR, IR, Polyisoprene) Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber.. |