Polymer Property : Shear Modulus = 0.0430 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0430 - 0.0430 GPa

@Temperature -12.0 - -12.0 °C
6.24 - 6.24 ksi

@Temperature 10.4 - 10.4 °F
Average value: 0.0430 GPa Grade Count:2
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..