Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0430 GPa @Temperature -12.0 °C |
6.24 ksi @Temperature 10.4 °F |
ASTM D1053 |
Precision Polymer Engineering V70D Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 70.Applications: Mouldings which are requ.. |
|||
Shear Modulus | 0.0430 GPa @Temperature -12.0 °C |
6.24 ksi @Temperature 10.4 °F |
ASTM D1053 |
Precision Polymer Engineering V75B Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F14, Z1, where Z1 = compressi.. |
|||
Shear Modulus | 0.0430 - 0.0430 GPa @Temperature -12.0 - -12.0 °C |
6.24 - 6.24 ksi @Temperature 10.4 - 10.4 °F |
Average value: 0.0430 GPa Grade Count:2 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |