Mechanical Properties Metric English Comments
Shear Modulus <= 0.000700 GPa
<= 0.102 ksi
Arlon 0.008" (0.2032 mm) Primerless Thermabond® Uncured Silicone (99990A008)
0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T..
Shear Modulus <= 0.000700 GPa
<= 0.102 ksi
Arlon 0.008" (0.2032 mm) Thermabond® Uncured Silicone (99510N008)
0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T..
Shear Modulus <= 0.000700 GPa
<= 0.102 ksi
Arlon 0.015" (0.381 mm) Primerless Thermabond® Uncured Silicone (99990A015)
0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038)..
Shear Modulus <= 0.000700 GPa
<= 0.102 ksi
Arlon 0.015" (0.381 mm) Thermabond® Uncured Silicone (99510N015)
0.015 in., ±0.001 (0.38 mm, ±0.038) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.015 in ±0.001(0.38 mm ± 0.038)..